Cold Heading Defects: Die Bursting and Tool Failure in Screw Production

09.10.26 07:35 AM - By Lydia - Comment(s)
Cold Heading Defects: Die Bursting and Tool Failure in Screw Production
In cold heading, tooling works under extreme pressure — a single heading stroke can exert hundreds of tons of force on the die. When a die can no longer withstand this load, it cracks or shatters entirely, a failure known as die ...

Cold Heading Defects: Eccentric Screw Heads and Off-Center Forming

09.10.26 07:35 AM - By Lydia - Comment(s)

Cold Heading Defects: Eccentric Screw Heads and Off-Center Forming
In cold heading, the screw head must be formed concentric with the shank. When concentricity is lost, the result is an eccentric head — the head sits off-center, the drive recess (such as a Phillips cross) is misaligned, or the bearin...

Cold Heading Defects: Insufficient Material in Screw Heads

09.10.26 07:35 AM - By Lydia - Comment(s)

Cold Heading Defects: Insufficient Material in Screw Heads
In fastener manufacturing, cold heading shapes screw heads through high-speed plastic deformation of metal wire. When the process parameters are not properly controlled, the head may form incompletely — a defect known as insufficient material...

Cold Heading Defects in Screw Manufacturing: Head Flash & Double-Layer Heads

09.10.26 07:35 AM - By Lydia - Comment(s)

Cold Heading Defects in Screw Manufacturing: Head Flash & Double-Layer Heads
In precision fastener production, cold heading forms screw heads in a single high-speed stroke. Even minor parameter deviations, however, can produce visible surface defects. Two of the most frequent issues are head flas...

Why do burrs appear on fastener screws?

09.10.26 07:35 AM - By Lydia - Comment(s)

Head burrs  — thin fins or flash of excess metal around the head periphery — are a common cold heading defect that causes serious trouble downstream. Burrs interfere with seating, damage mating surfaces, and can even cut assembly workers' fingers. Here's how we analyze and eliminate this defect...